At the invitation of Binzhou Bohai Piston Technology Department, our company together with Dr. Xiao from the Light Alloy Research Institute of Central South University went to Shandong province for the trial and technical communication of AlTi5C0.2 application in aluminum piston casting from November 6th to 8th.

20191202131156445644 20191202131082188218

 

Bohai Piston is domestic leading and global top four piston manufacturer. The management of the entire company, from casting and molding, to processing, storage, consistently clean, tidy, in perfect order.

 

The main purpose of this communication is to solve the short refinement effective time of the AlTiB in the refinement process and a series of problems caused by the aggregation and precipitation of TiB2.

 

The refinement process in the production of pistons takes a long time, which requires effective time and stability of grain refiner,however, TiB2 starts aggregation and precipitation only in about 15 minutes,which can't make effective refinement.In addition, the defected product and the damage to the later grinding tools caused by the agglomeration of TiB2, also bring a relatively negative impact on the piston production.

The AlTi5C0.2 of our company ideally solves the above problems.

 

This contrasting test and trial lasted for two days, and three repeated tests were conducted. Refine the target aluminum alloy AlSi12, prepare 200kg aluminum liquid per furnace, and feed AlTi5C0.2 by 2 ‰, 2 ‰, and 6 ‰ in three tests. The positions of feeding are respectively before purifying and degassing, after degassing and then stirring 2 Minutes, before purifying and degassing. The actual refinement time exceeds 120 minutes. Samples are taken every 20 minutes during the test, and a total of 6 samples are taken for each test.

 

Bohai Piston Technical Communication Service_

 

The test shows that adding AlTi5C0.2 to aluminum-silicon alloy (high silicon),2 ‰ addition rate will refine the alloy; 6 ‰ will have a better effect on alloy refinement (within 120 minutes), and contrasted with adding same ratio of Al-5Ti-1B (within 30 minutes of refining time), the effect is slightly better; feeding AlTi5C0.2 to the aluminum liquid for 2 hours, the refining effect does not decline significantly.

 

Bohai Pistons is continuing to make further test and proof to discusst he influence of AlTi5C0.2 on the thermal conductivity and other mechanical properties of aluminum pistons.

 

The technical communication servicehas achieved positive results in general, and has brought more optimized solutions to the refinement of the aluminum piston field. Sincerely looking forward to the early mass production and application of the AlTi5C0.2 refinement solution in the field of aluminum pistons, and wish Bohai Pistons to continue to lead the long voyage.